The heating temperature before hot rolling of oriented silicon steel should be increased to about 1400 °C, the temperature of the rolling mill should be about 1200 °C, the final rolling temperature...
DESCRIPTION
The heating temperature before hot rolling of oriented silicon steel should be increased to about 1400 °C, the temperature of the rolling mill should be about 1200 °C, the final rolling temperature should be controlled above 950 °C, and then the rapid water spray cooling below 550 °C was taken as a steel coil.
Category | Grain-Oriented Electrical Steel |
Standard | AISI, ASTM, BS, DIN, GB, JIS, EN |
Thickness | 0.2- 0.8 mm |
Width | 900-1250 mm |
Origin
|
China |
MOQ | 5 tons |
FAQ
1.Q:Are you trading or manufacturer?
A:We are manufacture with exporting rights.
2.Q:Could you supply samples?
A:Yes,we can.
3.Q:What’s your payment method?
A:T/T is the best payment, but also L/C is received.