In order to improve magnetic inductance performance and reduce hysteresis loss, the lower the content of harmful impurities in silicon steel, the better, and require a flat plate shape and good sur...
DESCRIPTION
In order to improve magnetic inductance performance and reduce hysteresis loss, the lower the content of harmful impurities in silicon steel, the better, and require a flat plate shape and good surface quality.
B50A400 steel Mechanical Properties
Grade |
Nominal thickness(mm) |
tensile strength L(N/mm2) |
Yield Strength L(N/mm2) |
Elongation L(%) |
Hardness HV1 |
Bending frequency (times) |
Stacking factor(%) |
B50A400 |
0.50 |
7.65 |
454 |
302 |
32 |
170 |
≥15 |
B50A400 steel sheet Electromagnetic induction standard
Grade |
Nominal thickness(mm) |
Theoretical density(kg/dm3) |
Maximum core loss P17/50 |
minimum magnetic induction(T) |
B50A400 |
0.50 |
7.65 |
4.00 |
1.63 |
Electrical steel has a history of hundreds of years, including Si < 0.5% electrical steel and Si content 0.5 ~ 6.5% of the two types of silicon steel, mainly used as a variety of motors, transformers and ballast cores, is an important indispensable soft magnetic alloy in the power, electronics and military industries.If you are interested in our products, please feel free to send us an email to inquire.